FDS5 by Hoya
Obsolete
Unknown
Environmentally Dangerous
FDS5 by Hoya is an obsolete optical glass. It transmits from 0.33 to 2.33 µm with an nd of 1.761804 and a Vd of 26.914901. It has dangerous environmental properties.
Refractive Index vs Wavelength
Refractive Index Calculator
dn/dλ vs Wavelength
dn/dλ Calculator
Abbe Number Calculator
Transmission vs Wavelength
No transmission data available.
Transmission Calculator
Optical Properties
Thermal Properties
Chemical Resistance
| Climatic Resistance | — |
|---|---|
| Stain Resistance | — |
| Acid Resistance | — |
| Alkali Resistance | — |
| Phosphate Resistance | — |
Similar Glasses (Other Manufacturers)
| Glass | Manufacturer | nd | Vd | Compare |
|---|---|---|---|---|
| D62-27 | Corning | 1.761802 | 26.90455 | |
| SF55 | Schott | 1.7618 | 26.950177 | |
| PBH25 | Ohara | 1.761797 | 27.107724 | |
| PBH25W | Ohara | 1.761797 | 27.107726 | |
| H-ZF12 | CDGM | 1.76182 | 26.607986 | |
| ZF12 | CDGM | 1.761822 | 26.555686 | |
| PBH14 | Ohara | 1.761819 | 26.553651 | |
| PBH14W | Ohara | 1.761819 | 26.553651 | |
| N-SF14 | Schott | 1.76182 | 26.53 | |
| SF14 | Schott | 1.76182 | 26.53 |