K-VC82(M) by Sumita
Preferred
Common
Environmentally Friendly
K-VC82(M) by Sumita is a preferred optical glass with a common melt frequency. It transmits from 0.32 to 2.00 µm with an nd of 1.75028 and a Vd of 45.4. It has low thermal expansion (CTE of 5.9×10⁻⁶/K) and average chemical resistance.
Refractive Index vs Wavelength
Refractive Index Calculator
dn/dλ vs Wavelength
dn/dλ Calculator
Abbe Number Calculator
Transmission vs Wavelength
Transmission Calculator
Optical Properties
Thermal Properties
| TCE -30/70°C (10-6/K) | 5.9 |
|---|---|
| TCE 100/300°C (10-6/K) | 8.0 |
| Thermal Conductivity (W/mK) | — |
| Heat Capacity (J/gK) | — |
$$\frac{dn}{dT} = \frac{n_0^2 - 1}{2\,n_0}\left[5.27 \times 10^{-6} + 2(1.73 \times 10^{-8})\,\Delta T + 3(-7.19 \times 10^{-11})\,\Delta T^2 + \frac{6.68 \times 10^{-7} + 2(9.93 \times 10^{-10})\,\Delta T}{\lambda - 0.203}\right]
\Delta T = T - T_0, \quad T_0 = 20\,°\text{C}$$
Chemical Resistance
| Climatic Resistance | 1 |
|---|---|
| Stain Resistance | — |
| Acid Resistance | 4 |
| Alkali Resistance | — |
| Phosphate Resistance | — |
Similar Glasses (Other Manufacturers)
| Glass | Manufacturer | nd | Vd | Compare |
|---|---|---|---|---|
| P-LAF37 | Schott | 1.7555 | 45.66 | |
| H-LAF3B | CDGM | 1.744 | 44.900027 | |
| LAF2 | Hoya | 1.744 | 44.9 | |
| LAF20 | Hoya | 1.744 | 44.872914 | |
| N-LAF2 | Schott | 1.74397 | 44.85 | |
| D44-45 | Corning | 1.744001 | 44.818533 | |
| LAM2 | Ohara | 1.743997 | 44.787528 | |
| S-LAM2 | Ohara | 1.743997 | 44.786431 | |
| LAF2 | Schott | 1.744002 | 44.719972 | |
| H-LAF6LA | CDGM | 1.757 | 47.711817 |